SK33 SK34 Fireclay Brick
MOQ: 5 tons
Description
Fireclay brick, also known as sintered brick, is a small artificial block material for construction. Fireclay brick is made of clay (including shale, coal gangue and other powder materials) as the main raw material, treated by mud, forming, drying and roasting, with solid and hollow respectively.
Press hole rate cent: solid brick (do not have hole or the brick with hole rate less than 25%), porous brick (hole rate is equal to or more than 25%), the dimension of hole is small and the brick with much quantity, often use at bearing place, intensity grade is taller. Hollow brick (hole rate is equal to or greater than 40%, the size of the hole is large and the number of bricks, often used for non-bearing parts, strength grade is low).
Solid brick and porous brick are used at bearing structural wall body more, hollow brick is used at blame bearing structural wall body more.

Features
Good high temperature fire resistance under load / Low thermal expansion at high temperatures / Lower impurity content
Application
Fireclay bricks are widely used in the lining of coke oven, glass kiln, cement rotary kiln, lime kiln, all kinds of incinerator, heating furnace, etc.

Physical And Chemical Indicators
|
Brand |
SK-32 |
SK-33 |
SK-34 |
SK-35 |
|
|
Refractoriness (SK) |
32 |
33 |
34 |
35 |
|
|
Apparent Porosity (%) |
26 |
24 |
23 |
23 |
|
|
Bulk Density (g/cm3) |
2.10 |
2.15 |
2.20 |
2.25 |
|
|
Cold Crushing Strength (MPa) |
20 |
30 |
35 |
40 |
|
|
@ 1,000℃ Thermal Linear Expansion(%) |
0.6 |
0.6 |
0.6 |
0.6 |
|
|
@ 1350℃ x 2hrs Permanent Linear Change (%) |
±0.5 |
±0.5 |
±0.3 |
±0.3 |
|
|
@0.2MPa Refractoriness Under Load (℃) |
1,250 |
1,300 |
1,350 |
1,380 |
|
|
Chemical Composition (%) |
Al2O3 |
35 |
38 |
40 |
46 |
|
Fe2O3 |
3.0 |
2.2 |
2.0 |
2.0 |
|
|
Main Applications |
Coke Oven Incinerator Glass Furnace Various Rotary Kiln Reheating Furnace Chemical Reactor Blast Furnace, Torpedo Car Non Ferrous Metal Furnace General Industrial Furnace etc. |
||||
Hot Tags: sk33 sk34 fireclay brick, China sk33 sk34 fireclay brick manufacturers, suppliers, factory, Fused Cast Alpha Beta Alumina Refractory, fire brick fire-resistant, alumina based refractory brick, Andalusite Brick, Silica Refractory fire Brick, conventional shaped fire clay brick