Magnesia Carbon Brick
video

Magnesia Carbon Brick

Magnesia carbon brick is made of high melting point alkaline oxide magnesium oxide (melting point 2800°C) and high melting point carbon materials that are difficult to be infiltrated by slag as raw materials, and various non-oxide additives are added.
MOQ:5 tons
Send Inquiry
Product Introduction
Description

 

 

Magnesia carbon brick is a kind of basic refractory brick and has high corrosion resistance. Its physical and chemical indicators are: Mg070~85%, C0~20% apparent porosity 3%, volume density 2.87g/cm3, compressive strength 40~50MPa, 1400C flexural strength 10~15MPa .The quality of magnesia has an extremely important influence on the performance of magnesium carbon bricks. It is a non-burning composite refractory material combined with a carbon binder.

 

The purity of magnesia has a significant impact on the slag resistance of magnesia carbon brick. The higher the magnesium oxide content, the lower the relative impurities, the lower the degree of silicate phase separation, the higher the degree of direct bonding of periclase, and the higher resistance to slag penetration and slag melting loss. The impurities in magnesia mainly include calcium oxide, silicon dioxide, and iron oxide. If the content of impurities is high, especially boron oxide compounds, it will adversely affect the refractoriness and high temperature performance of magnesia.

 

Features

 

Magnesia carbon brick has many excellent characters such as good high temperature resistance, strong slag resistance, good thermal shock resistance , low high temperature creep and so on.

Extended Service Life: Magnesite carbon Brick's resistance to thermal stress, corrosion, and wear translates into a prolonged service life, reducing downtime and maintenance costs.

Versatility: Its adaptability makes it suitable for diverse applications, from steelmaking and foundries to non-ferrous metal industries and beyond.

Optimized Performance: The combination of magnesia and carbon creates a refractory brick that excels in challenging environments, ensuring optimal performance in critical industrial processes.

Cost-Effective Solutions: Magnesium Carbon Brick's durability and performance contribute to cost savings over time, making it a judicious investment for industries requiring reliable refractory materials.

Magnesia Carbon brick

 

 

Application

 

Magnesia carbon brick is mainly used for lining of converters, AC electric arc furnaces, DC electric arc furnaces, and slag lines of ladle.

Mag-c brick finds extensive application in industries requiring robust refractory solutions, such as steelmaking, foundries, and non-ferrous metal production. It serves as linings in converters, ladles, electric arc furnaces, and other high-temperature equipment, providing essential thermal and chemical protection. Its versatility and unmatched resilience make Magnesite Carbon Brick a cornerstone in the realm of refractory materials, ensuring the longevity and efficiency of industrial processes in challenging thermal environments.

application

 

 

Physical And Chemical Indicators

 

EAF

 

Brand

 

Properties

Chemical content (%)

Apparent Porosity (%)

 

Bulk Density (g/cm3)

 

Cold Crushing

Strength (MPa)

HMOR (1400℃X0.5hr)

 

Main Application

 

MgO

FC

Al2O3

 

 

 

 

 

JEF 12SL

85

12

3

3

3.05

40

12

Slag Line

JEF 14HS

83

14

3

3

3.1

40

12

Hot Spot

JEF 12CS

85

12

3

3

3.05

42

12

Cold Spot

JEF 14DE

83

14

3

3

3.1

42

12

Door End

 

Productive Process

 

1.Magnesia carbon bricks Raw material quality control including physical and chemical testing.           
2.Crushing and grinding of bulk raw materials.
3. According to customer data sheet required to mixing Raw Material.
Pressing or shaping the green brick depend on different raw material and brick shape.
4.Dry the bricks at dryer kiln.
5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
6.The quality control department will inspect the finished refractory bricks random.

product-750-487

 

Packing And Shipping

 

Magnesia carbon bricks Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.