Alumina Ceramic Sagger
video

Alumina Ceramic Sagger

Alumina ceramics sagger is a ceramic material with a-Al2O3 as the main crystal.The main materials of saggers are cordierite-mullite, mullite, corundum-mullite, alumina, fused quartz or a composite of these materials.
MOQ<5TONS
Send Inquiry
Product Introduction
Products Description

 

Alumina ceramic Saggar is a kiln tool. in the process of firing porcelain, in order to prevent gas and harmful substances from damaging and defacing the body and glaze, porcelain and blank bodies are placed in containers made of refractory materials for roasting, which is the saggar. It is made of refractory mud of various specifications of the round bowl or cuboid, by high temperature roasting.

 

 

alumina ceramic sagger

 

Products Features

 

1. High temperature resistance: alumina ceramic saggars can withstand extreme temperatures without melting or deforming, ensuring the stability of the enclosed items during the firing process.
 
2. Chemical inertness: These saggars exhibit excellent resistance to chemical reactions, ensuring that the materials being processed remain unaffected by the surrounding environment.
 
3. Thermal shock resistance: They have good thermal shock resistance, preventing cracking or damage when subjected to rapid temperature changes.

 

Products Applications

 

1. Lithium battery: Lithium cobalt oxide, lithium manganese oxide, cobalt oxide, lithium iron phosphate.

2. Rare earth

3. Magnetic steel

4. Soft magnetic

5. Lighting arrester varistor

6. Electronic ceramics

 

Physical and Chemical Indicators

 

Property

Cordierite-Mullite

Mullite-Corundum

Al2O3 %

≥80

≥ 92

Sio2 %

≤ 18

≤ 5

Fe2O3 %

≤ 1.2

≤ 0.5

Density g/Cm3

≥ 2.6

≥ 3.7

Thermal Expansion 1000 C

6.5

7.8

Refractoriness C

≥ 1750

≥ 1850

Work Temperature

≤ 1450

≤1500

 