Calcium Hexaaluminate Insulation Brick
video

Calcium Hexaaluminate Insulation Brick

Calcium hexaaluminate lightweight refractory bricks are especially a high-quality refractory material for high-temperature kiln linings with low thermal conductivity, good stability in high-temperature reducing atmospheres, good resistance to alkali and slag erosion, and long life.
Send Inquiry
Product Introduction
Products Description

 

Calcium hexaaluminate insulation brick is a new type of insulation material with excellent insulation performance and environmental protection performance. This insulation material mainly uses aluminum oxide and calcium oxide as the main raw materials and is made through a specific process.

 

Products  composition

 

The content of calcium hexaaluminate insulation bricks refers to the content percentage of aluminum hexaaluminate and aluminum tetroxide in its main raw materials. Generally speaking, the higher the content of aluminum hexaaluminate in insulation calcium hexaaluminate bricks, the better the insulation performance.

However, in practical applications, the higher the content of insulation calcium hexaaluminate bricks, the better. Because too high a content will reduce its strength, leading to problems such as cracking during use. Therefore, choosing the appropriate content can better meet actual needs.

 

Products advantage

 

Calcium hexaaluminate insulation bricks have the following advantages compared with other insulation materials:

1. Good thermal insulation performance. Because its main raw material contains aluminum hexaaluminate, it has good thermal insulation properties and can reduce energy loss.

2. Good environmental protection. insulation Calcium hexaaluminate bricks have a simple production process, less production waste water and waste gas emissions, and have strong environmental performance.

3. Good safety. insulation Calcium hexaaluminate bricks are not easy to burn and do not produce toxic gases, thus ensuring people's safety.

 

Products Choose

 

When selecting calcium hexaaluminate insulation bricks, the following factors should be considered:

1. Regional climate conditions. The thermal insulation performance required under different climate conditions is different, so it is necessary to understand the local climate conditions and choose appropriate insulation materials.

2. Building structure. Different building structures require different insulation materials, which need to be considered comprehensively based on the actual situation.

3. Price and performance. Price is a matter of great concern to everyone, and insulation materials with reasonable prices and excellent performance should be selected.

In short, choosing insulation calcium hexaaluminate bricks with appropriate content and high quality can better ensure the insulation performance and safety of the building, and can also save energy and reduce energy consumption for people.

Hot Tags: calcium hexaaluminate insulation brick, China calcium hexaaluminate insulation brick manufacturers, suppliers, factory, Zirconia Hollow Ball Brick, refractory silica insulation brick, light weight silica brick, Hollow zirconia refractory bricks, lightweight refractory brick, furnace mullite insulation brick

Send Inquiry