It is a common problem that high alumina fire bricks return to alkali and become frosty. So how to solve this problem? Topower refractory staff will give you the corresponding solutions for your reference:

 

high alumina fire brick


1. Strictly control raw materials: In order to ensure the excellent performance of high alumina bricks, we must choose raw materials with high purity and avoid using raw materials containing soluble salts. Ensure the reliability of its quality from the source. At the same time, strict quality testing is carried out on raw materials to ensure that they meet relevant standards. This is like a comprehensive "physical examination" of bricks to ensure that they have a healthy "physique".

2. Optimize the firing process: In order to ensure the excellent performance of high alumina fire bricks, we need to accurately control the temperature and time during the firing process. Appropriately increasing the firing temperature and extending the firing time can promote the complete decomposition of soluble salts and avoid later frost problems. At the same time, we must also pay attention to the control of the firing atmosphere to avoid excessive oxidation atmosphere. An excessively oxidizing atmosphere will cause the crust to become tough. Therefore, only when the temperature, time and atmosphere are controlled just right, can we bake perfect high-alumina refractory bricks, making them always stable and efficient!

3. Strengthen storage and transportation management: In order to ensure the performance and appearance of high alumina fire bricks, we must pay special attention to the environmental humidity during storage and transportation. Avoid contact with moisture and salty substances and keep the environment dry. This is the most basic care for high alumina refractory bricks. When necessary, we will also put it in a sealed "protective suit" to ensure that it is not disturbed by the external environment.

4. Pretreatment before use: Before using high alumina fire bricks, in order to ensure their best performance, we need to pretreat them. Through pre-treatment methods such as drying and natural air drying, we can effectively remove moisture and salt substances attached to the surface of bricks. In this way, the high-alumina refractory bricks can be put into use in the best condition, showing their super fire-resistant performance!

5. Regular maintenance: In order to ensure the long-term stable operation of high alumina refractory bricks, we need to regularly check the atmosphere control device in the kiln. Provide regular maintenance services for high alumina refractory bricks and conduct comprehensive physical examinations. In this way, our high alumina fire bricks can always be in the best condition!
​