A new type of building fireproof board- fireproof calcium silicate board is gradually moving towards the general construction market.With the wide application of calcium silicate board, manufacturers of calcium silicate board waterproof and fireproof also emerge as the times require. However, these manufacturers vary in size from the quality of the plates. Compared with the ranking of the manufacturers, I believe that everyone wants to know more about this type of plate. Let’s take a look at it with the editor.
Fire-resistant calcium silicate board is a kind of lining board, grid that can be used in new residential buildings, warehouse residential buildings, sound-absorbing ceilings, poured walls, composite wall panels, marine partition panels, air ducts and industrial panels and billboards. High-quality fireproof board for floors and siding for interior projects such as tunnels.
Fireproof silicate calcium board and silicate calcium board waterproof have high strength, low thermal conductivity and good fire resistance. In addition, it also has other characteristics such as waterproof and thermal insulation. Medium density fireproof calcium silicate board can be used for indoor partition, ceiling, sound insulation, decoration, fire prevention and other projects, high density silicate calcium board waterproof can be used in outdoor or humid environment after special coating treatment. Silicate calcium board has low thermal conductivity and good thermal insulation performance. When rock wool is filled in the cavity of insulating silicate calcium board, the thermal insulation ability of 10cm thick partition wall is obviously better than that of ordinary brick wall. Due to the molecular structure of diatom mud itself, calcium silicate plate also has good sound insulation ability.Because products produced in different batches will have different models, the price of calcium silicate board needs to be based on the specific model of fire-resistant calcium silicate plate. There are many kinds of boards, so there are differences in price. Usually the price is around 25-120 yuan, and the price of super thick fireproof calcium silicate plate is a little more expensive.
The thickness of the silicate calcium board is 30mm, 24mm, 20mm, 15mm, 12mm, 8mm, 6mm, 5mm, etc., with a width of 1.22 meters, a length of 2.44 meters / 3 meters, and the internal materials of the plate 995 are free of asbestos, benzene and Other harmful substances are composed of natural mineral fibers, cellulose fibers, calcareous materials, and siliceous materials. Between 1.2 g/cm3 and 1.4 g/cm3.