Chamotte
MOQ: 5 tons
Description
The standard Al2O3 content of chamotte ore is 38%, after calcination the Al2O3 content is about 44%, and Fe2O3<2%. The composition is stable, the texture is uniform, the structure is dense, and the section is shell-shaped and white. The technical term is the first-grade hard clay clinker, the main chemical components are AL2O3 and SiO2, accompanied by a small amount of Fe2O3 and trace amounts of Na2O and K2O. The main mineral is kaolin.
The chamotte we call generally refer to CALCINED CLAY. The content of Al2O3 in the calcined is about 44%, and the content of Fe2O3 is not more than 2%. The composition is stable, the texture is uniform, the structure is dense, and the section is shell-shaped.
The common colors after high temperature calcination are: pure white, light gray, light yellow brown, and a small amount of brown iron sheet.
Features
Chamotte are not easily dispersed in water and have low plasticity. It have heat resistance and sinterability. After being calcined at high temperature, the scorched gem has the characteristics of stable volume, high strength and low water absorption.
Application
Chamotte are used in the production of advanced refractory materials, ceramics, aluminum silicate refractory fiber production and military industry.
It is widely used in metallurgy, casting, chemical, ceramics, electric power, machinery, petroleum and other industries.
Physical And Chemical Indicators
|
Properties & Brand |
YNS45 |
YNS45 |
YNS44 |
YNS44 |
YNS43 |
YNS42 |
YNS40 |
|
A |
B |
A |
B |
||||
|
AL2O3 % |
46 |
45 |
44 |
44 |
43 |
42 |
40 |
|
SiO2 % |
49-52 |
49-52 |
50-53 |
50-53 |
50 |
50 |
50 |
|
Fe2O3 % |
1 |
1.15 |
1.3 |
1.5 |
2 |
2.5 |
3 |
|
TiO2 % |
0.8 |
0.8 |
0.9 |
0.9 |
1 |
1.1 |
1.2 |
|
K2O+Na2O % |
0.3 |
0.3 |
0.4 |
0.4 |
0.4 |
0.5 |
0.5 |
|
CaO+MgO % |
0.5 |
0.5 |
0.5 |
0.5 |
0.5 |
0.6 |
0.7 |
|
Bulk density g/cm³ |
2.58 |
2.55 |
2.52 |
2.5 |
2.45 |
2.4 |
2.37 |
|
Refractoriness °C |
1780 |
1770 |
1760 |
1750 |
1740 |
1720 |
1710 |
Productive Process
1.Raw material quality control including physical and chemical testing.
2.crushing and grinding of bulk raw materials.
3.Packing after quality testing

Packing And Shipping
Packaging according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By 25kg kraft paper bags+sea fumigated wooden pallets