Runner Brick
video

Runner Brick

Runner brick is made of clay, shale, coal gangue or fly ash as the main raw materials, and are baked into bricks with solid or porosity not greater than the specified value and the external dimensions conform to the specified.
MOQ: 50 pieces
Send Inquiry
Product Introduction
Description


Runner brick is usually used in bottom casting and pouring steel. The reasons that affect the purity of steel are mainly divided into two categories:
1. It is caused by the steelmaking operation process;
2. It is caused by refractory materials for steelmaking, such as flowing steel bricks. When molten steel flows from the molten steel tank to the ingot mold, it must pass through the flowing steel bricks. Due to the high temperature of the molten steel, the flowing steel bricks will be impacted, which will cause the flow of steel. Part of the steel brick structure falls off, and at the same time the molten steel will interact with the flowing steel bricks, and the reaction products will be mixed into the molten steel, which will affect the quality of the steel ingot.
Good runner brick must have a good water running function to ensure that the water that penetrates can penetrate the water base in a timely and effective manner. Therefore, it is important to use cementitious materials mixed with steel or lime as the sand pad of the cast steel brick.
1. It should be washed medium coarse sand. Because of the prerequisite energy limit, the physical index of the sand of the cast steel brick cushion is not specified in this regard.Bedding requirements for runner brick:
2. The physical functions of other pouring steel bricks should meet the requirements of the standard.
3. It should be semi-dry sand. The humidity control method is to squeeze the mixture into a mass by hand. Of course, it will pass after loosening. Dryness and wetness are good for leveling the surface, reducing the fine density of Yang dust and mobilizing the cushion.

 

Application

 

Runner brick is applied in iron-making blast furnaces, steel-making converters, refining furnaces, electric furnaces and other drying equipment, muffle furnaces, etc. And also can be uesd as high temperature differential calorimeter.

application

 

 

Physical And Chemical Indicators

 

Index/brand N-1 N-2a N-2b N-3a N-3b N-4 N-5 N-6
Refractoriness ℃≥ 1750 1730 1730 1710 1710 1690 1670 1580
0.2Mpa load softening start temperature≥ 1400 1350 1350 1320 1320 1300 1300 1300
Reburning line change% 1400℃2h +0.1-0.4 +0.1-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5
1350℃2h +0.1-0.4 +0.1-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5 +0.2-0.5
Apparent porosity% ≤ 22 24 26 24 26 24 26 28
Normal temperature compressive strength Mpa℃≥ 30 25 20 20 15 20 15 15 

 

Productive Process

1.Raw material quality control including physical and chemical testing.           
2.Crushing and grinding of bulk raw materials.
3. According to customer data sheet required to mixing Raw Material.
Pressing or shaping the green brick depend on different raw material and brick shape.
4.Dry the bricks at dryer kiln.
5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
6.The quality control department will inspect the finished refractory bricks random.

product-750-487

 

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

product-750-591

Hot Tags: runner brick, China runner brick manufacturers, suppliers, factory, Refractory Zero Expansion Silica Bricks, High Alumina Sleeve refractories Brick, mullite lip refractory brick, refractory fire bricks for pizza ovens, used fire brick, Special Alumina Brick