Silica Mullite Brick
video

Silica Mullite Brick

Silica mullite bricks are baked products with high wear resistance after being pressed and molded using sillimanite, mullite, high alumina clinker as the main raw materials or other auxiliary materials.
Send Inquiry
Product Introduction
Products Description

Silica mullite bricks are high-quality refractory materials commonly used in the construction of furnaces and kilns.SiMo bricks are composed of silicon carbide (SiC) and molybdenum disilicide (MoSi2), which greatly enhances their high temperature resistance and chemical stability. The unique combination of these materials makes SiMo bricks ideal for use in extreme heat applications. They are designed to withstand high temperatures and harsh environments while maintaining their strength and durability.

 

Products Parameters

1. Bulk density: ≥2.7 g/cm³
2. Apparent porosity: ≤16%
3. Cold crushing strength: ≥100 MPa
4. Thermal conductivity: ≤15(W/m·K)
5. Maximum service temperature: 1800℃

Products Features

1. Excellent high-temperature resistance: Silica mullite bricks can withstand high temperatures up to 1800℃, making them ideal for use in high-heat applications.
2. Good chemical stability: SiMo bricks are resistant to most chemicals and corrosive substances, making them suitable for use in harsh chemical environments.
3. High strength and durability: SiMo bricks are highly dense and have excellent compressive strength, ensuring their durability and long-lasting performance.
4. High thermal conductivity: SiMo bricks have a high thermal conductivity rate, ensuring even heat distribution throughout the treated area.

product-750-400

Products Application

Silica mullite bricks are mainly used in high-heat applications such as furnace linings, electric furnaces, and kiln linings. They are also used in the production of non-ferrous metals, ceramics, and glass industries.

 