Magnesite Carbon Brick
video

Magnesite Carbon Brick

Magnesia and graphite are dead-burned or fused to create magnesite carbon brick, a resin-bonded brick. If necessary, antioxidant is also given. Thermal resistance, corrosion resistance, and spalling resistance are all strong points of magnesia carbon brick.
Send Inquiry
Product Introduction
Description


Magnesite carbon brick belongs to basic refractory fire bricks. MgO-C refractory bricks are widely used in the steel industry and exhibit great resistance to thermal shock and corrosion at high temperatures. It is the perfect refractory material due to its high melting point and resistance to hydration. Topower Refractory is one of best manufacturers of magnesia carbon bricks in China, which can provide high quality resistance MgO-C refractory bricks.

 

Features

 

What advantages does magnesite carbon brick has?

Good tolerance to high temperatures

High resistance against slag corrosion

Good conductivity and thermal shock resistance

Favorable heat stability

With high density

 

Magnesia Carbon brick

Application

 

Where is magnesite carbon brick used in?

Magnesia carbon bricks are widely employed in the production of steel, particularly in basic oxygen furnaces, electric arc furnaces, and the lining of steel ladles. It is widely used for lining steel ladles. It provides a protective barrier against molten steel and slag, and it can withstand the extreme temperature and chemical conditions inside the ladle.

application

 

 

Physical And Chemical Indicators

 

EAF
BrandProperties Chemical content (%) Apparent Porosity (%) Bulk Density (g/cm3) Cold Crushing
Strength (MPa)
HMOR (1400ºCX0.5hr) Main Application
MgO FC Al2O3
EAF 12 SL 85 12 3 3 3.05 40 12 Slag Line
EAF 14 HS 83 14 3 3 3.1 40 12 Hot Spot
EAF 12 CS 85 12 3 3 3.05 42 12 Cold Spot
EAF 14 DE 83 14 3 3 3.1 42 12 Door End

 

BOF
BrandProperties Chemical content (%) Apparent Porosity (%) Bulk Density (g/cm3) Cold Crushing
Strength (MPa)
HMOR (1400ºCX0.5hr) Main Application
MgO FC Al2O3
BOF 10 BI 86 10 4 3 3 45 12 Bottom
BOF 10 LC 84 12 4 3 3.05 45 12 Lower Cone
BOF 14 BL 83 14 3 3 3.1 45 10 Barrel
BOF 12 CP 85 12 3 3 3.05 50 10 Charge Pad
BOF 16 TN 80 16 4 3 3.1 45 14 Trunnion
BOF 15 TH 81 15 4 3 3.1 45 14 Tap Hole
BOF 14 TC 84 14 2 3 3.05 40 10 Top Cone