High Al2O3 Brick
video

High Al2O3 Brick

High Al2O3 Brick has more than 48% alumina oxide, used as high quality refractory materials. The more content of high alumina it has, the better resistance of refractory fire brick will have.
MOQ: 5 tons
Send Inquiry
Product Introduction
Description

 

 

High Al2O3 Brick is incredibly tough, sturdy, long-lasting refractory fire brick, which is with aluminum oxide contained more than 55% ,higher than fireclay bricks. Refractories made of alumina are popular in the heat processing industry because of their great resistance to oxidizing and reducing environments.

 

Features
 

What are the properties of high alumina bricks?

Because of its neutral refractory property, High Al2O3 Brick can withstand acid slag erosion. Over 1770°C, High Alumina fire bricks have high thermal stability and refractoriness. At 1770°C and above, it has a high heat resistance and temperature resistance. High alumina brick is extensively used in heat processing industries.

 

high alumina brick

 

Application

 

High Al2O3 Brick comes in a variety of grades and shapes to suit different applications, and they can be custom-designed to meet specific requirements. High alumina fire refractory rick that can be used to construct electric arc furnaces, glass kilns, cement rotary kilns, air furnaces, reverberatory furnaces, and rotary kiln linings. It can also be used as heat accumulating checker bricks, chock plugs for gating systems, nozzle bricks, and so on.

 

application

 

 

Physical And Chemical Indicators

 

Brand

Properties

SK-36

SK-37

SK-38

SK-40

Refractoriness (SK)

36

37

38

40

Apparent Porosity (%)

23

23

23

20

 Bulk Density (g/cm3)

2.30

2.35

2.40

2.65

 

Cold Crushing Strength (MPa)

45

50

52

70

@ 1,000℃

Thermal Linear Expansion(%)

0.6

0.6

0.6

0.6

@1,400℃x2hrs

Permanent Linear Change (%)

±0.3

±0.3

±0.3

±0.2

@0.2MPa

Refractoriness Under Load (℃)

1,420

1,450

1,500

1,550

 

Chemical

Composition (%)

Al2O3

50

60

72

80

Fe2O3

2.0

2.0

2.0

1.8