Isostatically Pressed SnO2 Electrode
MOQ:5 tons
Description
Isostatically Pressed SnO2 Electrode is made from high grade and purity Tin Oxide, and can alternative to traditional Molybdenum electrodes. Carefully selected additives are used to promote good sintering and give a dense product with exceptional electrical conductivity and refractory properties. When heated to a certain temperature, its conductivity increases exponentially, making it a good conductor. Using Isostatically Pressed SnO2 Electrode can also help avoid the discolouring that can sometimes occur with Molybdenum electrodes. All electrodes are isostatically pressed and doesn't contain recycled or reclaimed material to ensure excellent consistency and the high quality production. Each electrode is individually tested and approved before dispatch.
Features
Good conductor/ High-temperature conductive at a certain temperature / Large resistance value at room temperature /Good electrode material
Application
Isostatically Pressed SnO2 Electrode as an ideal material can be good use in fully electrical melting or electrically assisted heating glass furnaces.
Physical And Chemical Indicators
|
Item
|
Index |
||
|
SnO2-98 |
SnO2-96 |
||
|
Chemical Analysis(%) |
SnO2 |
98.5 |
96 |
|
ZrO2 |
- |
2 |
|
|
Physical Properties |
Apparent Porosity(%) |
4.5 |
4.5 |
|
Bulk Density (g/cm3) |
6.5 |
6.5 |
|
|
Cold pressing strength(Mpa) |
350 |
350 |
|
|
Room temperature resistance(Ω*cm) |
0.02 |
- |
|
|
Maximum Service Temperature (℃) |
1650 |
1650 |
|
Hot Tags: isostatically pressed sno2 electrode, China isostatically pressed sno2 electrode manufacturers, suppliers, factory, High Power Graphite Electrode, Fused Cast AZS Block, Isostatically Pressed SnO2 Electrode brick, Graphite fire resistance brick, Zirconia fire resistance brick, Graphite refractory brick