Zirconia brick is an insulating refractory product made of zirconia hollow spheres as the main raw material. The refractoriness is greater than 2400 ° C.
MOQ:5 tons
Send Inquiry
Product Introduction
Description

 

Zirconia bricks have the advantages of high mechanical strength, good thermal shock stability, and resistance to glass liquid corrosion. As the thermal conductivity of majority of other refractories  is much higher than zirconia refractories , zirconia brick is used as a high temperature insulating refractory. Zirconia refractory is one of the main refractory materials for glass furnaces because it is not easily wetted by molten glass and has a low reaction with molten glass.

 

Features

High temperature resistance / High performance to large thermal expansion coefficient and wear / Good resistance of chemically aggressive /

 

Application

 

The zirconia brick uesd as the bottom paving materials for electronical and special glass tanks

Used in the key position of E glass fiber melting furnace and electric glass furnaces

Used as high corrosion resistant burner blocks

 

Physical And Chemical Indicators

 

  Item Index
Iso-Pressed Zirconia Brick Light Weight High Zirconia Brick
ZHDB-IP-98 ZGSB-69 ZGSB-65 LZ-98
Dense Type Grain Type
Chemical Composition ZrO2 98(Stablizer Included) 98(Stablizer Included) 69 65.5 98(Stablizer Included)
Al2O3 - - - - -
SiO2 - - 29 33 -
TiO2 - - 1 - -
Physical Properties Apparent Porosity 1 16 8 1 45
Bulk Demsity 5.20 4.80 4.26 4.35 3.00
Cold Crushing Strength 500 100 250 350 20

 

Productive Process

1.Raw material quality control including physical and chemical testing.           
2.Crushing and grinding of bulk raw materials.
3. According to customer data sheet required to mixing Raw Material.
Pressing or shaping the green brick depend on different raw material and brick shape.
4.Dry the bricks at dryer kiln.
5.Put the bricks into the tunnel kiln to burning by higher temp from 1300-1800 deg.
6.The quality control department will inspect the finished refractory bricks random.

product-750-550

 

Packing And Shipping

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor   
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

product-750-600

Hot Tags: zirconia brick, China zirconia brick manufacturers, suppliers, factory, Isostatically Pressed SnO2 Electrode brick, Special Refractory Brick, Chrome Zirconia Corundum Brick, Silicon Carbide Brick, Zirconia refractory brick, Graphite fire resistance brick

Send Inquiry

whatsapp

Phone

E-mail

Inquiry