Mgo-cr Brick
video

Mgo-cr Brick

Magnesia chrome bricks are commonly used in the steel industry for the lining of electric furnaces, converters and other high-temperature equipment. Its main components are magnesium oxide and chromium oxide, which are fired into refractory materials with excellent high-temperature performance under appropriate proportions.
Send Inquiry
Product Introduction
Products Description

 

 

Mgo-cr bricks needs to meet the following requirements: chromium oxide content between 40-50%, magnesium oxide content between 45-55%, and other impurity content should be controlled at very low levels. The combustion performance indicators of materials should comply with national standards to ensure that emissions generated during the combustion process will not cause environmental pollution.

 

Products Advantage

 

1. Excellent strength: Magnesia Chrome Brick has high compressive strength, which helps it withstand high loads and pressure.

 

2. Thermal shock resistance: Mgo-cr brick has the ability to withstand rapid temperature changes without cracking.

 

3. Corrosion resistance: Magnesia Chrome Brick is resistant to chemical and physical corrosion, making it ideal for use in harsh industrial environments.

 

4. High-temperature resistance: The brick can withstand temperatures up to 1800°C, making it suitable for use in high-temperature applications.

 

magnesia chrome bricks

 

Products  Application

 

1. Steel industry: The magnesia chrome brick is used in the lining of blast furnaces, electric arc furnaces, converters, and other high-temperature equipment.

 

2. Cement industry: Mgo-cr brick is used in the kilns and furnaces used in cement production.

 

3. Glass industry: The brick is used in the melters and regenerators used in glass production.

 

4. Chemical industry: The brick is used in the reactors, furnaces, and incinerators used in chemical plants.

application

 

 
Products  Production Process

 

 

1. Raw material preparation: High-purity magnesia and chrome ore are prepared and mixed.

 

2. Molding: The mixture is molded into the desired shape and size.

 

3. Drying: The molded Mgo-cr brick is dried in a drying chamber.

 

4. Sintering: The brick is sintered at high temperatures to achieve the desired properties.

 

5. Quality control: The finished brick is inspected to ensure it meets the required standards.

product-750-487

Hot Tags: mgo-cr brick, China mgo-cr brick manufacturers, suppliers, factory, Magnesia Carbon Brick, MgO C bricks for steel industry, high peeling resistance mgo-c bricks, magnesite chrome block high chrome bricks, mgo high chrome bricks, chrome fire resistance brick

Send Inquiry

whatsapp

Phone

E-mail

Inquiry