Vacuum Insulation Panels
video

Vacuum Insulation Panels

Vacuum Insulation Panels (VIPs) consist of a rigid, highly-porous core material encased in a thin, gas-tight envelope. The core is typically made from materials like fumed silica or aerogel, which are evacuated to create a vacuum, significantly reducing heat transfer. This innovative design allows VIPs to achieve thermal conductivities as low as 0.004 W/(m·K), making them up to five times more effective than conventional insulation materials.
Send Inquiry
Product Introduction
vacuum insulation panels Description

 

Vacuum insulation panels vips are designed to offer exceptional thermal insulation performance. Their ultra-thin design allows for significant space savings, making them suitable for applications with limited space. The vacuum environment within the panel reduces heat transfer to a minimum, achieving thermal conductivities as low as 0.004 W/(m·K). This is significantly lower than conventional insulation materials like mineral wool and polyurethane foam, which have thermal conductivities of 0.044 W/(m·K) and 0.024 W/(m·K), respectively. VIPs are available in various sizes and thicknesses, typically ranging from 10 mm to 25 mm, to meet the specific needs of different applications.

 

Vacuum insulation Plate Production process

 

The manufacturing process of vacuum insulating panels VIPs involves several critical steps:
1. Core Material Selection: High-purity fumed silica or aerogel is selected for its low thermal conductivity and mechanical strength.
2. Core Formation: The core material is formed into a rigid, highly-porous structure.
3. Vacuum Creation: The core is placed inside a gas-tight envelope, which is then evacuated to create a vacuum.
4. Sealing: The envelope is sealed to maintain the vacuum, ensuring long-term thermal performance.
5. Quality Control: Each panel undergoes rigorous testing to ensure it meets the required thermal and mechanical standards.

 

vacuum insulating panel Characteristics:

 

1. Superior Thermal Insulation: Vacuum insulation panels provide thermal insulation performance up to five times better than conventional materials, with an R-value of 66 per inch.
2. Slim Design: The ultra-thin design of VIPs allows for significant space savings, making them suitable for applications where thickness is a critical factor.
3. Durability: VIPs are designed to maintain their thermal performance over long periods, with some panels offering a service life of up to 25 years.
4. Fire and Moisture Resistance: VIPs are non-combustible and highly resistant to water and mold, making them suitable for use in various environmental conditions.
5. Eco-Friendly: Many VIPs are made from recycled materials and do not emit toxic gases, contributing to environmental sustainability.

 

nano board

 

Vacuum insulation Plate parameter

 

Brand

Property

JC950

JC1000

JC1100

Melting Point (℃)

≥1200

≥1200

≥1200

Operating Temperature (℃)

950

1000

1100

Density (kg/m³)

280-350

550-650

550-650

Compressive strength (MPa)

0.5

0.8-1.2

0.8-1.2

800℃

Heating wire shrink 800℃ (%)

≤1.9

≤1.9

≤1.9

 

 

Thermal Conductivity

(w/m.k)

 

 

 

 

200℃

0.016

/

/

400℃

0.021

0.043

0.047

600℃

0.026

0.057

0.058

800℃

0.035

0.063

0.069

 

namo insulation panels Application

 

Vacuum insulation panels are used in a variety of applications due to their superior thermal insulation properties:
- Building Construction: Used in exterior wall insulation, flat roofs, and prefabricated buildings to enhance energy efficiency.
- Refrigeration and Cold Chain Logistics: VIPs maintain consistent temperatures in refrigerated containers and transportation systems, reducing energy consumption.
- Industrial Thermal Management: Used in high-temperature equipment and blast furnace pipes to reduce heat loss.
- Special Environments: VIPs are used in cold storage, LNG carriers, and renovation projects for their ability to withstand extreme temperatures and conditions.

Hot Tags: vacuum insulation panels, China vacuum insulation panels manufacturers, suppliers, factory, Microporous Board, Ceramic Fiber Cotton Bulk, Ceramic Fiber Bulk, 1500c Ceramic Fiber Blanket, Cordierite Mullite Insulation Brick, Stainless Steel Anchor