Corundum Refractory Castable
Products Description
Corundum Refractory Castable is a high-grade refractory castable that is widely used in furnace applications. It is mainly composed of high-purity corundum aggregates, superfine powder, and binder. It also includes other additives that promote bonding, sintering, and densification. The materials are blended in a specific ratio, depending on the application requirement and manufacturing conditions.

|
Product Name: |
Corundum Refractory Castable |
| Appearance: | White Powder |
| Main Raw Material: | Corundum, high-alumina cement, mullite, etc. |
| Max Service Temperature: | 1750°C |
| Bulk Density (g/cm³): | 2.7-2.9 |
| Cold Crushing Strength (MPa): | ≥80 |
| Thermal Conductivity (W/m.K): | 1.3-1.5 |
| Refractoriness (°C): | ≥1750 |
| Water Consumption for Construction (%): | 6-8 |
Products Features
Corundum Refractory Castable is a superior refractory material that offers the following features:
1. High purity
2. High strength
3. Excellent resistance to thermal shock
4. High abrasion and erosion resistance
5. High density
6. Excellent resistance to chemical attack
7.Good mechanical and thermal properties.
8.Excellent thermal stability
Products Process
Corundum Refractory Castable includes mixing, molding, drying, and firing. The materials are mixed in a specific proportion, and water is added to form a slurry. The slurry is then poured into a mold and vibrated to remove any trapped air. The molded shape is then dried and fired at high temperatures to create the final product.
Products Advantage
1. Corundum Refractory Castable is resistant to high temperatures and thermal shock, making it ideal for use in a variety of high-temperature applications.
2. The high strength of this castable ensures that it will withstand high-temperature and high-pressure conditions.
3. Its excellent abrasion and erosion resistance make it suitable for use in harsh industrial environments.
4. The high purity and density of this product make it a reliable and long-lasting refractory material.
Products Application
Corundum Refractory Castable is an ideal choice for using in steel, cement and other industries. It is a reliable, high-strength, high-density, and long-lasting refractory material that offers exceptional resistance to thermal shock, abrasion, and erosion. Thus, it is the preferred choice for many industries that require high-temperature applications.
It is widely used in metallurgy, cement plants, power plants, and other industries. It is used in the construction of various furnace linings, such as electric furnaces, ladles, and tundishes, and can be used in high-temperature environments up to 1800°C.
Hot Tags: corundum refractory castable, China corundum refractory castable manufacturers, suppliers, factory, Non-stick Aluminum Castable, insulating castable refractory cement, insulating castable, Monolithic Refractory, Anti Crust Refractory Castable, Anti Skinning Castable refractory
Previous
Silica Ramming MassYou Might Also Like
Send Inquiry