Silica Ramming Mass
Products Description
https://youtu.be/C6YDHvNl82c
Silica Ramming Mass is a refractory lining material primarily composed of high-purity silica. Through advanced technology, it undergoes a rigorous process, ensuring uniform grain size distribution and superior thermal stability. This technology results in a product that can withstand extreme temperatures and harsh chemical environments.
Products Characteristics
The material exhibits outstanding characteristics, including high melting point, minimal thermal expansion, excellent thermal shock resistance, and exceptional erosion and corrosion resistance. Its consistent composition ensures structural stability under demanding conditions, making it an ideal choice for various industrial applications.
silica ramming mass also have excellent environmental performance. It uses natural minerals as raw materials and does not produce any harmful substances or pollutants during the production process. Moreover, silica ramming materials will not release harmful substances during use, and will not cause any harm to the environment or human health. This makes it a very ideal green and environmentally friendly material that meets the high requirements of modern society for environmental performance.
|
Silica Ramming Mass |
Indexes |
|
SiO2, % ≥ |
90 |
|
Fe2O3, % ≤ |
2 |
|
BD, g/cm3 ≥ |
2 |
|
Refractoriness, ℃ ≥ |
1750 |
|
Strength at normal temp, MPa ≥ |
2 |
|
Cold crushing strength, MPa ≥ |
10 |
Products Procss
Silica Ramming Mass is meticulously manufactured using a controlled process that involves precise blending, mixing, and controlled grain sizing of high-purity silica. This process guarantees a product with uniform density, minimized impurities, and superior thermal properties, meeting stringent quality standards.
Products Advantage
High Thermal Stability: With an ability to withstand extreme temperatures, our Silica Ramming Mass ensures durability and reliability in demanding industrial furnaces and reactors.
Excellent Erosion and Corrosion Resistance: Its robust composition resists chemical attacks, ensuring prolonged service life and reduced maintenance costs.
Low Thermal Expansion: Minimal expansion under heat prevents cracks and structural damage, ensuring consistent performance over time.
Consistent Quality: Rigorous quality control measures guarantee uniformity in composition and performance, meeting the exacting standards of industrial applications.
Products Application
Silica Ramming Mass finds extensive use in various industries, including steelmaking, non-ferrous metal industries, glass manufacturing, and more. It serves as a lining material in induction furnaces, coreless induction furnaces, and other high-temperature applications, ensuring efficient and reliable operation.
Product Application Instructions:
For optimal performance, it is crucial to ensure proper application:
Preparation: Clean the furnace or reactor surface thoroughly to remove any contaminants.
Mixing: Use the recommended mixing ratios and apply the Silica Ramming materials evenly, compacting it uniformly within the lining.
Ramming: Employ suitable ramming techniques to achieve the desired density and eliminate voids.
Baking: Gradually heat the lining to the recommended temperature to cure the material effectively.