What are the differences between high alumina bricks and magnesia bricks?

High alumina bricks are aluminum-silicon series products, and magnesia bricks are magnesia series products. High aluminum bricks can resist weak alkali and weak acid atmospheres and are neutral products; magnesia refractory bricks resist strong alkali erosion and cannot be used in acidic atmospheres and are alkaline. series of products.
1. High alumina bricks and magnesia bricks are two different materials
High alumina refractory bricks and magnesite bricks are two refractory products with different materials and properties. The density of magnesium bricks is above 3.0 and the melting point is 2850°C. The density of high alumina fire bricks is above 2.3 and the melting point is 1500°C.
2. Description of raw materials and refractoriness of magnesia bricks
The raw materials of magnesite refractory bricks are magnesia particles ranging from less than 5 mm to fine powder, which are crushed, formed, and sintered at a high temperature of 1600°C. The raw materials of high alumina bricks are alumina particles and fine powder, which are crushed, formed, and sintered at a high temperature of 1450°C. Made by sintering.
The refractoriness of magnesia bricks is above 2000℃, and the load resistance is 1800℃. However, magnesium refractory bricks have high thermal conductivity and poor thermal shock resistance. High temperature resistance. Magnesia bricks have poor resistance to acidic slag and cannot be in direct contact with acidic products. If they are in the kiln lining with acidic products, they must be separated by high alumina bricks before they can be used. Moreover, magnesium bricks have poor hydration resistance and tend to grow white hair when exposed to water. They also produce cracks and reduce their strength. Magnesium fire bricks must be protected from moisture, rain and snow during storage and transportation.
3. What is the fire resistance of high alumina bricks?
The refractoriness of high aluminum bricks is above 1700℃. The load softening temperature is 1520℃ and does not exceed 1600℃. The load softening temperature of high alumina firebricks also varies greatly according to different raw material grades. The load softening temperature of grade three high aluminum fire bricks is still around 1410°C. Although high alumina bricks are neutral bricks, they have good thermal shock stability, are not afraid of hydration, and can be used in weakly alkaline and weakly acidic atmospheres.
Therefore, at different temperatures in different kiln linings, the selection of magnesia bricks or high alumina refractory bricks must be based on the degree of corrosion and atmosphere. Magnesite fire bricks must be selected in alkaline atmospheres. The use temperature is below 1400°C, and weak alkali bricks are used. Or in a weak acid atmosphere, high alumina fire bricks can be used.
The difference between high alumina bricks and magnesite refractory bricks is that they have different materials, different operating temperatures, different corrosion-resistant atmospheres, and different thermal shock effects. Another difference is the market price. The price of high alumina refractory bricks is low and the price of magnesia bricks is high.