SK34 Firebrick
MOQ<5TONS
Products Description
SK34 firebrick is premium-quality clay refractory brick highly regarded for their ability to withstand high temperatures. It find widespread usage in industries requiring reliable materials for furnace linings, kilns, and other high-heat applications.
"SK": This is a common naming method for refractory bricks, used to identify the type of brick. Different letter and number combinations represent different fire resistance properties and uses. "34": This is the grade or grade of SK34 fire bricks. SK34 usually indicates medium fire resistance and is suitable for use under moderate temperature and pressure conditions. SK34 refractory fire bricks are typically able to withstand temperatures of approximately 1300 degrees Celsius to 1400 degrees Celsius.Therefore, refractory SK34 firebricks are usually used for the lining of industrial furnaces, sintering furnaces, heat treatment furnaces, sintering furnaces and other high-temperature equipment requiring moderate refractory properties.
Products Parameters
|
Brand |
SK-34 |
|
|
Refractoriness (SK) |
34 |
|
|
Apparent Porosity (%) |
23 |
|
|
Bulk Density (g/cm3) |
2.20 |
|
|
Cold Crushing Strength (MPa) |
35 |
|
|
@ 1,000℃ Thermal Linear Expansion(%) |
0.6 |
|
|
@ 1350℃ x 2hrs Permanent Linear Change (%) |
±0.3 |
|
|
@0.2MPa Refractoriness Under Load (℃) |
1,350 |
|
|
Chemical Composition (%) |
Al2O3 |
40 |
|
Fe2O3 |
2.0 |
|
SK34 firebrick primary raw materials include high-grade refractory clays and other additives. These materials are carefully selected and processed to achieve optimal properties, such as high-temperature stability, mechanical strength, and resistance to thermal shock.
The manufacturing process involves blending the selected raw materials into a homogenous mixture, forming the mixture into brick shapes through molding or pressing, and firing them at high temperatures. This firing process ensures the development of robust and heat-resistant structures in the bricks.
Products Features
High Thermal Stability: SK34 firebricks exhibit remarkable resistance to high temperatures, maintaining structural integrity and stability in extreme heat environments.
Resistance to Thermal Shock: They demonstrate exceptional resilience against rapid temperature changes, crucial for applications involving thermal cycling.
Appropriate Porosity: SK34 clay fire bricks have controlled apparent porosity, offering a balance between insulation and mechanical strength, ensuring resistance to thermal stress and wear.
Superior Mechanical Strength: They possess robust mechanical properties, including high compressive strength and resistance to abrasion, ensuring durability and long service life in harsh conditions.

Products Application
SK34 clay refractory bricks are widely employed in various industries, primarily as linings in furnaces, kilns, and reactors. They play a critical role in providing thermal insulation and stability required in high-temperature environments, ensuring efficient and reliable industrial operations.
SK34 firebrick Used as linings for steelmaking converters, ladles, and tundishes due to their high-temperature resistance and ability to endure thermal cycling, contributing to efficient steel production in Steel Industry,Cement and Lime Kilns,Glass Manufacturing,Ceramics Industry .

Hot Tags: sk34 firebrick, China sk34 firebrick manufacturers, suppliers, factory, Zircon Aggregate fire resistance Bricks, heating furnace refractory brick fire cla, Alumina Refractory Anchor Brick, clay brick, Corundum Mullite Composite refractory Brick, Chromium Zirconium Mullite Brick