Slide Gate Refractory Plate
Products Description
The key raw ingredients for the Slide Gate Refractory Plate are tabular alumina, carbon material, and zirconia-containing material. High performance antioxidants were also used. Phenolic resin was employed as a binder, and the plates were formed under high pressure and burned at high temperatures.
The number of Slide Gate Refractory can be divided into two layers and three layers according to the number of skateboards. The two -layer skateboards are not moving on the skateboard, and the sliding plate follows the followers to slide. Most of the two -layer skateboards are used on the steel bag mechanism. The three -layer skateboards are not moving on the upper and sliding plates. The middle skateboard follow -up portfolio slides to control and adjust the effect of steel water flow; most of the three -layer skateboards are mostly used on the middle bag mechanism.
There are two types of sliding water mouths: straight lines and rotating types. At present, most of the steel factories at home and abroad use linear institutions, and there are fewer applications for rotating institutions.

Features
The Slide Gate Refractory Plate has the advantages of higlh strength,good erosion resistance,thermal shock resistance and good stability etc,mainly used in large,medium and small size ladles. The classification of skateboards is not the same. According to the material process, it is divided into aluminum carbon skateboards, pyrine skateboards, aluminum carbon skateboards, magnesium skateboards, metal binding skateboards, and high aluminum skateboarding; Middle temperature is fired for skateboarding, without burning skateboarding.
Physical And Chemical Indicators
|
Brand & Properties |
Ladle Nozzle |
Ladle Slide Gate Plate |
|
|
Chemical Composition (%) |
Al2O3 |
≥75 |
≥80 |
|
C |
≥6 |
≥6 |
|
|
Bulk Density (g/cm3) |
≥2.7 |
≥3.0 |
|
|
Apparent Porosity (%) |
≤18 |
≤14 |
|
|
Cold Crushing Strength (MPa) |
≥45 |
≥90 |
|

Application
Alumina Slide Gate Refractory Plate: This skateboard uses high -purity aluminum powder as the main raw material, which is processed by multiple processes such as forming, drying, sintering, and other processes. It has excellent high temperature resistance and chemical stability, and is widely used in high -temperature furnace kiln.
Silicate skateboarding: This kind of skateboard is made of silicate material. It has excellent high temperature resistance and corrosion resistance. It is suitable for high -temperature equipment in the metallurgy and power industries.
Silicon carbide skateboarding: silicon carbide material has high hardness and high temperature resistance, and is an ideal refractory material. Silicon carbide skateboarding is widely used in high -temperature production fields such as glass and ceramics, and can effectively protect equipment from high temperature erosion.
In short, Slide Gate Refractory Plate is an important industrial refractory and insulation material. According to different applications and requirements, you can choose products made of different materials.
Hot Tags: Slide Gate Refractory Plate, China Slide Gate Refractory Plate manufacturers, suppliers, factory, Ladle Shroud, Zirconia Ceramic Nozzle Inserts, Sliding Gate Plate, Refractory Crucible, Zirconia Ceramic Inserts, Porous Plug And Seat Well Block
Previous
Zirconia InsertNext
Zircon NozzleYou Might Also Like
Send Inquiry