Tundish Stopper
MOQ: 100 pieces
Description
Tundish stopper is composed of rod core, sleeve brick and plug brick. The rod core is usually made of plain carbon steel round steel with a diameter of 30-60mm. The upper end is connected with the cross arm of the lifting mechanism by bolts, the lower end is connected with the plug brick by threads or pins, and the middle sleeve brick. Tundish stopper must be carefully built and used after baking and drying for more than 48 hours to avoid breakout accidents caused by refractory explosions.
The integral stopper rod is installed in the tundish when in use. The flow rate of molten steel entering the mold can be adjusted by controlling the position of the stopper rod head to the tundish nozzle, and argon can also be blown to the tundish through the argon blowing hole to prevent the nozzle from being blocked.
Features
Good erosion resistance / Corrosion resistance / Stable flow control during casting / Close tightly after casting
Application
Tundish stopper is widely used in ladle, refined ladle, electric furnace refined ladle, tundish.
Physical And Chemical Indicators
|
Brand / Properties
|
Tundish Stopper |
|||||||
|
Body |
Slag Line |
Head |
||||||
|
Chemical Composition (%) |
Al2O3 |
53.28 |
-- |
86.61 |
71.43 |
15.1 |
||
|
Fe2O3 |
0.91 |
-- |
0.43 |
0.91 |
-- |
|||
|
SiO2 |
14.48 |
-- |
0.77 |
10.65 |
8.95 |
|||
|
TiO2 |
1.41 |
-- |
0.33 |
-- |
-- |
|||
|
ZrO2 |
-- |
75.1 |
-- |
-- |
0.29 |
|||
|
CaO |
-- |
1.71 |
-- |
-- |
1.56 |
|||
|
MgO |
-- |
-- |
-- |
5.71 |
56.8 |
|||
|
LOI (%) |
30.59 |
15.01 |
11.11 |
10.95 |
17.3 |
|||
|
Bulk Density (g/cm3) |
2.42 |
3.78 |
2.85 |
2.78 |
2.59 |
|||
|
Apparent Porosity (%) |
14.3 |
15.61 |
17.7 |
17.7 |
16.7 |
|||
|
Fracture Strength (MPa) |
8.4 |
6.97 |
6.73 |
6.73 |
7.8 |
|||
|
Main Application |
Ladle & Tundish |
|||||||
Hot Tags: tundish stopper, China tundish stopper manufacturers, suppliers, factory, Zirconia Ceramic Inserts, Ladle Shroud, Tundish Nozzle, Refractories Nozzle, Refractory Ladle Slide Gate Plate, zirconia nozzle composite tundish metering nozzle
Previous
Ladle ShroudYou Might Also Like
Send Inquiry