Silicon Carbide Castable
video

Silicon Carbide Castable

Silicon carbide castable is a castable refractory material composed of corundum or high-aluminum clinker, silicon carbide, carbon, binders and admixtures. It is mainly used as the lining of the blast furnace tap trough, so it is also called tap trough refractory Castable。
Send Inquiry
Product Introduction
Products Description

silicon carbide castables

Silicon carbide castables, due to the high hardness of SiC (Mohs hardness 9.2, expansion coefficient not greater than 4.4 It has good corrosion resistance, high high temperature strength, high thermal conductivity, small linear expansion coefficient, good thermal shock resistance, does not react with cement raw materials, and has good skinning resistance.

 
Products Parameters

 

product name Silicon carbide castable
AI2O3% 50
SiO2+SiC% 40
Volume density g/cm3 ≥2.5
Cold pressing strength 110°CX24h MPa ≥80
Flexural strength 110°CX24hMPa ≥8
After burning at 1300℃ ≥8
Line change rate after burning: 1300°CX3h ±0.3
Application area Decomposition furnace cone and kiln tail smoke chamber

 

Products Features

 

1. High refractoriness: Silicon carbide has high refractoriness and can maintain stable performance for a long time in high temperature environments above 1600°C.

2. Oxidation resistance: Silicon carbide castables have good antioxidant properties at high temperatures and can resist the erosion of oxidizing media such as oxygen and water vapor.

3. Corrosion resistance: Silicon carbide has excellent acid and alkali resistance and can effectively resist erosion by corrosive substances such as slag and metal oxides.

4. Wear resistance: Silicon carbide has high hardness and excellent wear resistance, and can resist wear under harsh conditions such as high temperature, high pressure and flowing media.

5. Good thermal conductivity: Silicon carbide has high thermal conductivity, which is beneficial to the rapid transfer and uniform distribution of heat in the furnace, and improves the thermal efficiency of the furnace equipment.

6. Easy to construct: Silicon carbide castable has good fluidity and can be poured, sprayed or tamped easily, simplifying the construction process.

 

Products Application

 

Silicon carbide castables mainly use silicon carbide as the main raw material, add water reducing agent and ultrafine powder, and use pure calcium aluminate cement as the binding agent, which can greatly reduce the number of skinning times and is suitable for preheater unloading of large and medium-sized dry cement kilns. Slopes, rising flues, decomposition furnace cones and other parts.

 