White Corundum is a ceramic material with extremely high fire resistance that can withstand the working environment under harsh conditions such as high temperature, high voltage, high speed, and high load.
Send Inquiry
Product Introduction
Products Description

 

White Corundum uses industrial aluminum powder as the raw material, which is cooled after melting at high temperature above 2000 degrees in the arc. It is a type of artificial abrasive. The content of tritenuxide (AL2O3) is more than 99%, and it contains a small amount of iron oxide, silicon oxide and other ingredients, which are white. Its texture is dense and hard. Product size is produced in accordance with international standards and national standards, which can be processed according to user requirements

 

Features

 

High melting point and high softness point: The melting point is 2050 ° C, and the softening point is above 1800 ° C, so it can withstand very high temperature.

Good seismic resistance and vibration resistance: White Corundum has excellent seismic resistance and vibration resistance, making it excellent in high -speed rotation or vibration equipment.

Excellent corrosion resistance: It can resist the corrosion of most acid and alkali, so it can be used in some environments with high requirements for corrosion resistance.

Good wear resistance: The hardness of White Aluminum Oxide is very high, which can effectively prevent damage caused by wear and wear.

Low thermal expansion coefficient: The thermal expansion coefficient is very small, so you can maintain a stable form and size under high temperature conditions.

 

Application

 

White Corundum is widely used in the manufacturing of refractory materials, such as: high temperature furnace, heat insulation material, insulation material, casting mold, refractory brick, fire resistance coating, etc. In these applications, Bai Gangyu can not only maintain stable performance, but also to withstand extreme temperature and pressure. It has very strong anti -oxidation, corrosion resistance, and abrasion resistance. It provides important technical support and for industrial production and provides important technical support and Assure.

 

 

Physical And Chemical Indicators

 

Loss of Ignition (%) 0.3
Chemical Composition (%) Al2O3 ≥98.9
SiO2 ≤0.10
Fe2O3 ≤0.20
Na2O ≤0.49
K2O ≤0.03
MgO ≤0.01
CaO ≤0.09

 

 

Packing and Shipping

 

Packaging  according to safety sea-exporting packing Standard
Dispatch : loading the finished packing material at factory by container Door toDoor
By sea fumigated wooden pallet + plastic belt  + plastic film wrap.

product-750-600

Hot Tags: white corundum, China white corundum manufacturers, suppliers, factory, Alumina Tabular Alumina White Corundum, bauxite for refractory, dead burned magnesia, abrasive powder corundum, calcined alumina powder, Chamotte

Send Inquiry

whatsapp

Phone

E-mail

Inquiry