Glass Melting Furnace Mullite Insulation Brick Chemical Corrosion Resistance High temperature mullite insulation bricks for sale are made from good quality and superior raw materials with...
Mullite Bricks are manufacture with mullite as the main raw material through molding and firing in the high temperature. Its refractoriness is higher up to...
Mullite Insulation Brick Features 1. Low thermal conductivity 2.High cold crushing strength 3.Perfect Energy saving 4.Stable volume 5.Excellent heat insulation 6.High intensity for...
The physical and chemical properties of a typical corundum-mullite brick are: Al2O3>85%, Fe2O3 0.45%, apparent porosity 19%, normal temperature compressive strength is greater than...
Light Weight Mullite Insulation Brick, mainly based on aluminum silicate-based refractory materials, with some excellent performance, (especially high temperature creep performance)...