China Alkali resistant refractory castable Manufacturers Factory Suppliers
Alkali resistant castable refractory for intermediate frequency furnace to acidic aluminium silicate refractory castable for intermediate frequency .The characteristics of alkali resistant...
Light alkali resistant castables has high strength and low body density are mainly used for alkali resistant insulation lining in areas with alkali corrosion in kiln. Working Hours Mon - Fri 10 to 5pm...
May 29, 2020 · Alkali resistant refractory castable is a kind of alkali resistant castable made of aluminum silicate as refractory aggregate and powder and made of aluminate cement...
Mar 20, 2017 · Al2O3 Content: 48% Shape:: Powder Bulk Density:: 2.1g/cm3 Cold Modules Of Rupture:: 7MPa Max Service Temperature:: 1300℃ Permanent Linear Change:: ±0.4 Alkali-Resistance:: Grade 1 Cold...
Alkali resistant castable has good high temperature performance and alkali corrosion resistance.It can form a glaze layer on the surface of the material in a high temperature...
Alkali-resistant castable use alumina silicate materials as aggregate and powder, configured with alumina cement and admixture. It reacts with alkali metal oxide at high temperature to form a high...